Home > Stainless Steel > UNS S21603 datasheet,UNS S21603 chemical,UNS S21603 heat treatment

UNS S21603 datasheet,UNS S21603 chemical,UNS S21603 heat treatment
2019-08-15 12:48:05   Source:   Criticism:0 CTR:

This page provides UNS S21603 stock,UNS S21603 datasheet,UNS S21603 mechanical properties, UNS S21603 chemical element,UNS S21603 performance specifications.
Chemical Composition (Weight %)
C (%) ≤ 0.03
Si(%) ≤ 0.75
Mn(%) 7.50~9.00
P(%) ≤ 0.045
S (%) ≤ 0.030
Cr (%) 17.5 ~ 22.0
Ni (%) 5.00 ~ 7.00
Mo(%) 2.00 ~3.00
Other (%) 0.25 ~ 0.50
Mechanical Properties
Condition of heat treatment -
Tensile Rm (MPa) 690
Yield Rp0.2 (MPa) 415
Elongation A (%) 40.0
Reduction in cross section on fracture Z (%) -
Impact AKV/AKU (J) -
Brinell Hardness (HBW) 100 max
The alloy is usually produced by BEF & AOD followed by electroslag remelting (ESR) / VAR if necessary for special purpose.
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Bars are usually supplied black/bright in the annealed condition.
Forms and Shapes:
Round bar (Diameter): 5.50 ~ 650mm
Square bar / Flat bar: 3 ~ 650mm
Wire rod (Diameter): 0.10 ~ 16mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 650mm X L (or in coil form)