This page provides ASTM 201 datasheet, ASTM 201 mechanical properties, chemical element ASTM 201, technical specifications of ASTM 201 steel material properties. ASTM 201 performance specifications.
Chemical Composition (Weight %)
C (%) ≤ 0.15
Si(%) ≤ 1.00
Mn(%) 5.05~7.50
P(%) ≤ 0.060
S (%) ≤ 0.030
Cr (%) 16.0 ~ 18.0
Ni (%) 3.50 ~ 5.50
Mo(%) -
Other (%) N ≤ 0.25
Mechanical Properties
Condition of heat treatment -
Tensile Rm (MPa) 655
Yield Rp0.2 (MPa) 310
Elongation A (%) 40.0
Reduction in cross section on fracture Z (%) -
Impact AKV/AKU (J) -
Brinell Hardness (HBW) 240 max.
The alloy is usually produced by BEF & AOD followed by electroslag remelting (ESR) / VAR if necessary for special purpose.
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Bars are usually supplied black/bright in the annealed condition.
Forms and Shapes:
Round bar (Diameter): 5.50 ~ 650mm
Square bar / Flat bar: 3 ~ 650mm
Wire rod (Diameter): 0.10 ~ 16mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 650mm X L (or in coil form)